Description

Molybdenum is transformed into TZM (Titanium-Zirconium-Molybdenum) by using small quantities of tiny, extremely fine carbides. TZM is stronger than pure molybdenum and possesses a higher recrystallization temperature and better creep resistance.

This material data has been provided by Plansee.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Thermal

PropertyValue

Max service temperature

1400 °C

Show Supplier Material materials with Max service temperature of 1400 °C

Chemical properties

PropertyValue

Aluminium

1E-4 %

Show Supplier Material materials with Aluminium of 1E-4 %

Cadmium

1E-4 %

Show Supplier Material materials with Cadmium of 1E-4 %

Chromium

3E-4 %

Show Supplier Material materials with Chromium of 3E-4 %

Copper

2E-4 %

Show Supplier Material materials with Copper of 2E-4 %

Iron

5E-4 %

Show Supplier Material materials with Iron of 5E-4 %

Molybdenum

balance

Nickel

1E-4 %

Show Supplier Material materials with Nickel of 1E-4 %

Nitrogen

5E-4 %

Show Supplier Material materials with Nitrogen of 5E-4 %

Oxygen

0.01 %

Show Supplier Material materials with Oxygen of 0.01 %

Potassium

6E-4 %

Show Supplier Material materials with Potassium of 6E-4 %

Silicon

2E-4 %

Show Supplier Material materials with Silicon of 2E-4 %

Titanium

0.4 - 0.55 %

Show Supplier Material materials with Titanium of 0.4 - 0.55 %

Tungsten

0.02 %

Show Supplier Material materials with Tungsten of 0.02 %

Zirconium

0.06 - 0.12 %

Show Supplier Material materials with Zirconium of 0.06 - 0.12 %

Technological properties

Property
Application areas

TZM is used in high-temperature applications involving demanding mechanical loads, for example in forging tools or as rotating anodes in X-ray tubes. The recommended temperatures of use are between 700 and 1400 °C.