Thermal
Property | Value |
---|---|
Max service temperature | 1400 °C Show Supplier Material materials with Max service temperature of 1400 °C |
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % |
Chromium | 3E-4 % Show Supplier Material materials with Chromium of 3E-4 % |
Copper | 2E-4 % Show Supplier Material materials with Copper of 2E-4 % |
Iron | 5E-4 % Show Supplier Material materials with Iron of 5E-4 % |
Molybdenum | balance |
Nickel | 1E-4 % Show Supplier Material materials with Nickel of 1E-4 % |
Nitrogen | 5E-4 % Show Supplier Material materials with Nitrogen of 5E-4 % |
Oxygen | 0.01 % Show Supplier Material materials with Oxygen of 0.01 % |
Potassium | 6E-4 % Show Supplier Material materials with Potassium of 6E-4 % |
Silicon | 2E-4 % Show Supplier Material materials with Silicon of 2E-4 % |
Titanium | 0.4 - 0.55 % Show Supplier Material materials with Titanium of 0.4 - 0.55 % |
Tungsten | 0.02 % Show Supplier Material materials with Tungsten of 0.02 % |
Zirconium | 0.06 - 0.12 % Show Supplier Material materials with Zirconium of 0.06 - 0.12 % |
Technological properties
Property | ||
---|---|---|
Application areas | TZM is used in high-temperature applications involving demanding mechanical loads, for example in forging tools or as rotating anodes in X-ray tubes. The recommended temperatures of use are between 700 and 1400 °C. |