General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 10.2 g/cm³ Show Supplier Material materials with Density of 10.2 g/cm³ |
Molar mass | 95.94 g/mol Show Supplier Material materials with Molar mass of 95.94 g/mol | |
Neutron capture cross-section | 23.0 °C | 0 m² Show Supplier Material materials with Neutron capture cross-section of 0 m² |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 320 GPa Show Supplier Material materials with Elastic modulus of 320 GPa | |
Hardness, Vickers, 10 | 23.0 °C | 160 - 180 [-] Show Supplier Material materials with Hardness, Vickers, 10 of 160 - 180 [-] | recrystallized |
Poisson's ratio | 23.0 °C | 0.31 [-] Show Supplier Material materials with Poisson's ratio of 0.31 [-] |
Thermal
Property | Temperature | Value |
---|---|---|
Boiling point | 4639 °C Show Supplier Material materials with Boiling point of 4639 °C | |
Coefficient of thermal expansion | 23.0 °C | 5.2E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5.2E-6 1/K |
Melting point | 2620 °C Show Supplier Material materials with Melting point of 2620 °C | |
Specific heat capacity | 23.0 °C | 254 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 254 J/(kg·K) |
Thermal conductivity | 23.0 °C | 142 W/(m·K) Show Supplier Material materials with Thermal conductivity of 142 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 1.79E+7 S/m Show Supplier Material materials with Electrical conductivity of 1.79E+7 S/m |
Electrical resistivity | 23.0 °C | 5.6E-8 Ω·m Show Supplier Material materials with Electrical resistivity of 5.6E-8 Ω·m |
Electron work function | 23.0 °C | 4.39 eV Show Supplier Material materials with Electron work function of 4.39 eV |
Acoustical
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % |
Carbon | 1.3E-3 % Show Supplier Material materials with Carbon of 1.3E-3 % |
Chromium | 3E-4 % Show Supplier Material materials with Chromium of 3E-4 % |
Copper | 2E-4 % Show Supplier Material materials with Copper of 2E-4 % |
Iron | 5E-4 % Show Supplier Material materials with Iron of 5E-4 % |
Molybdenum | 99.97 % Show Supplier Material materials with Molybdenum of 99.97 % |
Nickel | 1E-4 % Show Supplier Material materials with Nickel of 1E-4 % |
Nitrogen | 5E-4 % Show Supplier Material materials with Nitrogen of 5E-4 % |
Oxygen | 6E-4 % Show Supplier Material materials with Oxygen of 6E-4 % |
Potassium | 6E-4 % Show Supplier Material materials with Potassium of 6E-4 % |
Silicon | 2E-4 % Show Supplier Material materials with Silicon of 2E-4 % |
Tungsten | 0.02 % Show Supplier Material materials with Tungsten of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | Molybdenum can be used, for example, to produce ribbons and wires for the lighting industry, semiconductor base plates for power electronics, glass melting electrodes, hot zones for high-temperature furnaces and sputtering targets for coating solar cells and flat screens. |