General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 16.6 g/cm³ Show Supplier Material materials with Density of 16.6 g/cm³ |
Molar mass | 180.95 g/mol Show Supplier Material materials with Molar mass of 180.95 g/mol | |
Neutron capture cross-section | 23.0 °C | 0 m² Show Supplier Material materials with Neutron capture cross-section of 0 m² |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 186 GPa Show Supplier Material materials with Elastic modulus of 186 GPa | |
Hardness, Vickers, 10 | 23.0 °C | 80 - 125 [-] Show Supplier Material materials with Hardness, Vickers, 10 of 80 - 125 [-] | recrystallized |
Poisson's ratio | 23.0 °C | 0.35 [-] Show Supplier Material materials with Poisson's ratio of 0.35 [-] |
Thermal
Property | Temperature | Value |
---|---|---|
Boiling point | 5458 °C Show Supplier Material materials with Boiling point of 5458 °C | |
Coefficient of thermal expansion | 23.0 °C | 6.4E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 6.4E-6 1/K |
Crystallization temperature | 900 - 1450 °C Show Supplier Material materials with Crystallization temperature of 900 - 1450 °C | |
Melting point | 2996 °C Show Supplier Material materials with Melting point of 2996 °C | |
Specific heat capacity | 23.0 °C | 140 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 140 J/(kg·K) |
Thermal conductivity | 23.0 °C | 57.5 W/(m·K) Show Supplier Material materials with Thermal conductivity of 57.5 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 8.00E+6 S/m Show Supplier Material materials with Electrical conductivity of 8.00E+6 S/m |
Electrical resistivity | 23.0 °C | 1.3E-7 Ω·m Show Supplier Material materials with Electrical resistivity of 1.3E-7 Ω·m |
Electron work function | 23.0 °C | 4.3 eV Show Supplier Material materials with Electron work function of 4.3 eV |
Superconductive transition temperature | -268.65 °C Show Supplier Material materials with Superconductive transition temperature of -268.65 °C |
Acoustical
Technological properties
Property | ||
---|---|---|
Application areas | Tantalum's corrosion resistance makes it a valuable material in a large number of chemical applications. This material is used, for example, to produce heat exchangers for the equipment construction sector, charge carriers for furnace construction, implants for medical technology and capacitor components for the electronics industry. |