The material: 'Densimet® D185ND Tungsten Heavy Alloy Turned Rod 70 mm' you were looking for has been superseded by the one below.

Densimet® D185ND Tungsten Heavy Alloy Turned Rod

Want to keep this datasheet? Save it now in your required format

Description

Plansee Densimet® composite materials are heavy metals with a high tungsten content (> 90%) and a NiFe binder phase.

Related Standards

Equivalent Materials

This material data has been provided by Plansee.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

18.25 - 18.85 g/cm³

Show Supplier Material materials with Density of 18.25 - 18.85 g/cm³

Dimension

PropertyValue

Diameter

30 - 70 mm

Show Supplier Material materials with Diameter of 30 - 70 mm

Length

250 - 500 mm

Show Supplier Material materials with Length of 250 - 500 mm

Dimensions

Available dimensions (diameter x length, mm x mm): 30 x 500; 40 x 500; 70 x 250

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

2 %

Show Supplier Material materials with Elongation of 2 %

Hardness, Vickers, 10

23.0 °C

270 - 330 [-]

Show Supplier Material materials with Hardness, Vickers, 10 of 270 - 330 [-]

Tensile strength

23.0 °C

689 MPa

Show Supplier Material materials with Tensile strength of 689 MPa

Yield strength Rp0.2

23.0 °C

517 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 517 MPa

Chemical properties

PropertyValue

Iron

0.5 - 1.5 %

Show Supplier Material materials with Iron of 0.5 - 1.5 %

Nickel

1.5 - 2.5 %

Show Supplier Material materials with Nickel of 1.5 - 2.5 %

Tungsten

96 - 98 %

Show Supplier Material materials with Tungsten of 96 - 98 %

Technological properties

Property
Application areas

Densimet® tungsten alloys are distinguished by their particularly high density. Combined with their ability to absorb radiation as well as their outstanding mechanical properties and machinability, they are the ideal materials for a wide range of applications, such as in aerospace, the automotive industry, medical engineering and the construction industry.

Other

Weakly ferromagnetic, DENSIMET® D185ND is according to RoHS directives (EU2002/95/EG, EU2000/53/EG, EU2006/122/EG) and REACH Regulation EC 1907/2006.