General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 16.9 - 17.6 g/cm³ Show Supplier Material materials with Density of 16.9 - 17.6 g/cm³ |
Dimension
Property | Value |
---|---|
Diameter | 10 - 40 mm Show Supplier Material materials with Diameter of 10 - 40 mm |
Length | 250 - 500 mm Show Supplier Material materials with Length of 250 - 500 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 10 x 250; 12 x 250; 16 x 250; 20 x 500; 25 x 500; 30 x 500; 40 x 500 |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 360 GPa Show Supplier Material materials with Elastic modulus of 360 GPa |
Elongation | 23.0 °C | 4 - 18 % Show Supplier Material materials with Elongation of 4 - 18 % |
Hardness, Rockwell C | 23.0 °C | 31 [-] Show Supplier Material materials with Hardness, Rockwell C of 31 [-] |
Hardness, Vickers, 10 | 23.0 °C | 300 - 360 [-] Show Supplier Material materials with Hardness, Vickers, 10 of 300 - 360 [-] |
Tensile strength | 23.0 °C | 800 - 990 MPa Show Supplier Material materials with Tensile strength of 800 - 990 MPa |
Yield strength | 23.0 °C | 700 MPa Show Supplier Material materials with Yield strength of 700 MPa |
Yield strength Rp0.2 | 23.0 °C | 550 MPa Show Supplier Material materials with Yield strength Rp0.2 of 550 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 5.3E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5.3E-6 1/K |
Thermal conductivity | 500.0 °C | 65 W/(m·K) Show Supplier Material materials with Thermal conductivity of 65 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Iron | 1.5 - 2.5 % Show Supplier Material materials with Iron of 1.5 - 2.5 % |
Molybdenum | 3.5 - 4.5 % Show Supplier Material materials with Molybdenum of 3.5 - 4.5 % |
Nickel | 3.5 - 4.5 % Show Supplier Material materials with Nickel of 3.5 - 4.5 % |
Tungsten | 88.5 - 91.5 % Show Supplier Material materials with Tungsten of 88.5 - 91.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Densimet® tungsten alloys are distinguished by their particularly high density. Combined with their ability to absorb radiation as well as their outstanding mechanical properties and machinability, they are the ideal materials for a wide range of applications, such as in aerospace, the automotive industry, medical engineering and the construction industry. | |
Other | Weakly ferromagnetic, DENSIMET® D2M is according to RoHS directives (EU2002/95/EG, EU2000/53/EG, EU2006/122/EG) and REACH Regulation EC 1907/2006. |