General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 16.6 g/cm³ Show Supplier Material materials with Density of 16.6 g/cm³ |
Neutron capture cross-section | 23.0 °C | 0 m² Show Supplier Material materials with Neutron capture cross-section of 0 m² |
Dimension
Property | Value |
---|---|
Diameter | 4 - 10 mm Show Supplier Material materials with Diameter of 4 - 10 mm |
Length | 300 - 2500 mm Show Supplier Material materials with Length of 300 - 2500 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 4 x 500-2000 ; 6 x 500-2500 ; 10 x 300-2500 |
Mechanical
Thermal
Property | Value |
---|---|
Crystallization temperature | 900 - 1450 °C Show Supplier Material materials with Crystallization temperature of 900 - 1450 °C |
Melting point | 2966 °C Show Supplier Material materials with Melting point of 2966 °C |
Electrical
Property | Temperature | Value |
---|---|---|
Electron work function | 23.0 °C | 4.3 eV Show Supplier Material materials with Electron work function of 4.3 eV |
Superconductive transition temperature | -268.65 °C Show Supplier Material materials with Superconductive transition temperature of -268.65 °C |
Acoustical
Chemical properties
Property | Value | Comment |
---|---|---|
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % | |
Carbon | 1E-3 % Show Supplier Material materials with Carbon of 1E-3 % | |
Hydrogen | 4E-4 % Show Supplier Material materials with Hydrogen of 4E-4 % | |
Iron | 5E-4 % Show Supplier Material materials with Iron of 5E-4 % | |
Molybdenum | 1E-3 % Show Supplier Material materials with Molybdenum of 1E-3 % | |
Nickel | 5E-4 % Show Supplier Material materials with Nickel of 5E-4 % | |
Niobium | 1.9E-3 % Show Supplier Material materials with Niobium of 1.9E-3 % | |
Nitrogen | 5E-4 % Show Supplier Material materials with Nitrogen of 5E-4 % | |
Oxygen | 1.3E-3 % Show Supplier Material materials with Oxygen of 1.3E-3 % | |
Silicon | 1E-3 % Show Supplier Material materials with Silicon of 1E-3 % | |
Tantalum | 99.95 % Show Supplier Material materials with Tantalum of 99.95 % | min |
Titanium | 1E-4 % Show Supplier Material materials with Titanium of 1E-4 % | |
Tungsten | 2E-3 % Show Supplier Material materials with Tungsten of 2E-3 % |
Technological properties
Property | ||
---|---|---|
Corrosion properties | Outstanding resistance against aqueous solutions and metal melts. | |
Other | This material has excellent cold ductility, superconductivity and a high level of biocompatibility. |