General
Property | Value | Temperature |
---|---|---|
Density | 16.6 g/cm³ Show Supplier Material materials with Density of 16.6 g/cm³ at 23.0 °C | 23.0 °C |
Neutron capture cross-section | 0 m² Show Supplier Material materials with Neutron capture cross-section of 0 m² at 23.0 °C | 23.0 °C |
Dimension
Property | Value |
---|---|
Diameter | 0.5 - 2 mm Show Supplier Material materials with Diameter of 0.5 - 2 mm |
Dimensions | Available diameters (mm): 0.5; 0.8; 1; 1.5; 2 |
Mechanical
Property | Value | Temperature |
---|---|---|
Elongation | 15 % Show Supplier Material materials with Elongation of 15 % at 23.0 °C | 23.0 °C |
Thermal
Property | Value |
---|---|
Crystallization temperature | 900 - 1450 °C Show Supplier Material materials with Crystallization temperature of 900 - 1450 °C |
Melting point | 2996 °C Show Supplier Material materials with Melting point of 2996 °C |
Electrical
Property | Value | Temperature |
---|---|---|
Electron work function | 4.3 eV Show Supplier Material materials with Electron work function of 4.3 eV at 23.0 °C | 23.0 °C |
Superconductive transition temperature | -268.65 °C Show Supplier Material materials with Superconductive transition temperature of -268.65 °C |
Acoustical
Chemical properties
Property | ||
---|---|---|
Cadmium | 1E-3 % | |
Carbon | 5E-3 % | |
Chromium | 1E-3 % | |
Hydrogen | 1.5E-3 % | |
Iron | 5E-3 % | |
Lead | 1E-3 % | |
Mercury | 1E-3 % | |
Molybdenum | 5E-3 % | |
Nickel | 5E-3 % | |
Niobium | 0.01 % | |
Nitrogen | 5E-3 % | |
Oxygen | 0.02 % | |
Silicon | 5E-3 % | |
Tantalum | 99.95 % | min |
Titanium | 1E-3 % | |
Tungsten | 2E-3 % |
Technological properties
Property | ||
---|---|---|
Corrosion properties | Outstanding resistance against aqueous solutions and metal melts. | |
Other | This material has excellent cold ductility, superconductivity and a high level of biocompatibility. |