Description

White S-B-S thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish.

This material data has been provided by Primeline Polymers.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

0.95 g/cm³

Show Supplier Material materials with Density of 0.95 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

20.0 °C

345 %

Show Supplier Material materials with Elongation of 345 %

ASTM D412

Hardness, Shore A

20.0 °C

50 [-]

Show Supplier Material materials with Hardness, Shore A of 50 [-]

ASTM D2240

Modulus at 100% elongation

20.0 °C

1.9 GPa

Show Supplier Material materials with Modulus at 100% elongation of 1.9 GPa

ASTM D412

Tear strength

20.0 °C

22.1 kN/m

Show Supplier Material materials with Tear strength of 22.1 kN/m

ASTM D624

Tensile strength

20.0 °C

3.4 MPa

Show Supplier Material materials with Tensile strength of 3.4 MPa

ASTM D412

Technological properties

Property
Application areas

Elastocon® 3353 is heat sealable and well suited for consumer goods and extruded tubing and profile applications.

Other

Elastocon® 3353 thermoplastic elastomer compound does not require drying. Elastocon® concentrates are not compatible with flexible PVC and should not be blended with or used in an application where direct contact is intended. It can be overmolded and/or coextruded onto polystyrene.

Processing methods