RADITECK P RV400K 1700 NT

Alternative and trade names
PPS-GF40, PPS-T GF40
Want to keep this datasheet? Save it now in your required format

Description

PPS 40% glass fibre reinforced injection moulding grade. Heat stabilized. Natural colour with Balanced matching of excellent chemical resistance, inherent flame retardancy and very good heat ageing properties retention. Suitable for parts requiring very high stiffness and high mechanical strength.

This material data has been provided by Radici Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.63 g/cm³

Show Supplier Material materials with Density of 1.63 g/cm³

dry

ISO 1183

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

15 GPa

Show Supplier Material materials with Elastic modulus of 15 GPa

dry

ISO 527-2/1A

1mm/min

Elongation

2 %

Show Supplier Material materials with Elongation of 2 %

dry

ISO 527-2/1A

5mm/min

Flexural modulus

14 GPa

Show Supplier Material materials with Flexural modulus of 14 GPa

dry

ISO 178

2mm/min

Flexural strength

275 MPa

Show Supplier Material materials with Flexural strength of 275 MPa

dry

ISO 178

2mm/min

Impact strength, Charpy notched

23 °C

10 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m²

dry

ISO 179/1eA

Impact strength, Charpy unnotched

23 °C

40 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 40 kJ/m²

dry

ISO 179/1eU

Impact strength, Izod notched

-40 °C

11 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 11 kJ/m²

ISO 180/1A

23 °C

11 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 11 kJ/m²

ISO 180/1A

Thermal

PropertyValueTesting StandardPressureComment

Coefficient of thermal expansion

1.6e-05 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.6e-05 1/K

ISO 11359-1/-2

23°C-55°C

4.6e-05

Show Supplier Material materials with Coefficient of thermal expansion of 4.6e-05

ISO 11359-1/-2

23°C-55°C, Transverse

Heat deflection temperature

265 °C

Show Supplier Material materials with Heat deflection temperature of 265 °C

ISO 75/2Af

2 MPa

270 °C

Show Supplier Material materials with Heat deflection temperature of 270 °C

ISO 75/2Bf

0.45 MPa

Melting point

280 °C

Show Supplier Material materials with Melting point of 280 °C

ISO 11357-1/-3

10°C/min

Flammability

Class: V-0 ,method: UL 94, and thickness tested (mm): 0.8

Electrical

PropertyValueConditionTesting StandardComment

Comparative tracking index

150 V

Show Supplier Material materials with Comparative tracking index of 150 V

dry

IEC 60112

Sol.A

Rheological Properties

PropertyValueTesting StandardConditionComment

Melt mass-flow rate

124 g/10min

Show Supplier Material materials with Melt mass-flow rate of 124 g/10min

ISO 1133

315°C/5Kg

Shrinkage

0.6 %

Show Supplier Material materials with Shrinkage of 0.6 %

ISO 294-4

dry

Technological properties

Property
Certifications

RoHS 2011/65/UE

Color

Natural

Fillers

40% Glass Fiber

Processing methods

Injection Molding