PA66 flame retardant injection moulding grade. Halogen and phosphorus free. Black colour.

Suitable for parts where fire retardancy is required. Rated V-0 at 0.4 mm according to UL-94. Also suitable for monofilament extrusion.

This material data has been provided by Radici Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting StandardThickness

Density

1.18 g/cm³

Show Supplier Material materials with Density of 1.18 g/cm³

dry

ISO 1183

Limiting oxygen index

32 %

Show Supplier Material materials with Limiting oxygen index of 32 %

ISO 4589-2

Moisture absorption

1.8 %

Show Supplier Material materials with Moisture absorption of 1.8 %

50% RH

ISO 62

2 mm

Water absorption

7.7 %

Show Supplier Material materials with Water absorption of 7.7 %

ISO 62

2 mm

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

4 GPa

Show Supplier Material materials with Elastic modulus of 4 GPa

dry

ISO 527-2/1A

1mm/min

Elongation

3 %

Show Supplier Material materials with Elongation of 3 %

dry

ISO 527-2/1A

50mm/min

Flexural modulus

4 GPa

Show Supplier Material materials with Flexural modulus of 4 GPa

dry

ISO 178

2mm/min

Flexural strength

115 MPa

Show Supplier Material materials with Flexural strength of 115 MPa

dry

ISO 178

2mm/min

Impact strength, Charpy notched

23 °C

4 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m²

dry

ISO 179/1eA

Impact strength, Charpy unnotched

23 °C

30 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 30 kJ/m²

dry

ISO 179/1eU

Yield strength

71 MPa

Show Supplier Material materials with Yield strength of 71 MPa

dry

ISO 527-2/1A

50mm/min

Thermal

PropertyValueTesting StandardThicknessPressureComment

Ball pressure temperature

200 °C

Show Supplier Material materials with Ball pressure temperature of 200 °C

IEC 60695-10-2

Glow Wire Flammability Index

960 °C

Show Supplier Material materials with Glow Wire Flammability Index of 960 °C

IEC 60695-2-12

1 mm, 2 mm

Glow Wire Ignition Temperature

725 °C

Show Supplier Material materials with Glow Wire Ignition Temperature of 725 °C

IEC 60695-2-12

2 mm

800 °C

Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C

IEC 60695-2-13

1 mm

Heat deflection temperature

70 °C

Show Supplier Material materials with Heat deflection temperature of 70 °C

ISO 75/2Af

2 MPa

200 °C

Show Supplier Material materials with Heat deflection temperature of 200 °C

ISO 75/2Bf

0.45 MPa

Melting point

260 °C

Show Supplier Material materials with Melting point of 260 °C

ISO 11357-1/-3

10°C/min

Vicat softening temperature

220 °C

Show Supplier Material materials with Vicat softening temperature of 220 °C

ISO 306

50°C/h 50N

Flammability

Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 | Class: V-0 ,method: UL 94, and thickness tested (mm): 0.4

Electrical

PropertyValueConditionTesting StandardComment

Comparative tracking index

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

dry

IEC 60112

Sol.A

Surface resistivity

1e+10 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq

50%RH

IEC 60093

500V

1e+12 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq

dry

IEC 60093

500V

Volume resistivity

1e+12 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm

50%RH

IEC 60093

500V

1e+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm

dry

IEC 60093

500V

Rheological Properties

PropertyValueConditionTesting StandardComment

Shrinkage

1.1 %

Show Supplier Material materials with Shrinkage of 1.1 %

dry

ISO 294-4

1.1 %

Show Supplier Material materials with Shrinkage of 1.1 %

dry

ISO 294-4

Transverse

Technological properties

Property
Certifications

RoHS 2011/65/UE

Color

Black

Processing methods

Injection Molding