RADILON DT 40EP25W X18213 BK

Alternative and trade names
PA612
Want to keep this datasheet? Save it now in your required format

Description

PA612 flexible, high viscosity extrusion grade. Toughened and plasticized, heat stabilized. Black colour

Suitable for extrusion of profiles, tubes and pipes.

This material data has been provided by Radici Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting StandardThickness

Density

1.03 g/cm³

Show Supplier Material materials with Density of 1.03 g/cm³

dry

ISO 1183

Moisture absorption

0.8 %

Show Supplier Material materials with Moisture absorption of 0.8 %

50% RH

ISO 62

2 mm

Water absorption

2.1 %

Show Supplier Material materials with Water absorption of 2.1 %

ISO 62

2 mm

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

0.9 GPa

Show Supplier Material materials with Elastic modulus of 0.9 GPa

dry

ISO 527-2/1A

1mm/min

Elongation

120 %

Show Supplier Material materials with Elongation of 120 %

dry

ISO 527-2/1A

50mm/min

Elongation at yield

30 %

Show Supplier Material materials with Elongation at yield of 30 %

dry

ISO 527-2/1A

Flexural modulus

0.85 GPa

Show Supplier Material materials with Flexural modulus of 0.85 GPa

dry

ISO 178

2mm/min

Flexural strength

31 MPa

Show Supplier Material materials with Flexural strength of 31 MPa

dry

ISO 178

2mm/min

Impact strength, Charpy notched

23 °C

80 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 80 kJ/m²

dry

ISO 179/1eA

Yield strength

34 MPa

Show Supplier Material materials with Yield strength of 34 MPa

dry

ISO 527-2/1A

50mm/min

Thermal

PropertyValueTesting StandardComment

Melting point

210 °C

Show Supplier Material materials with Melting point of 210 °C

ISO 11357-1/-3

10°C/min

Flammability

Class: HB ,method: UL 94, and thickness tested (mm): 3

Electrical

PropertyValueConditionTesting StandardComment

Surface resistivity

1e+10 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq

50%RH

IEC 60093

500V

1e+12 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq

dry

IEC 60093

500V

Volume resistivity

1e+12 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm

50%RH

IEC 60093

500V

1e+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm

dry

IEC 60093

500V

Technological properties

Property
Certifications

RoHS 2011/65/UE

Color

Black

Processing methods

Injection Molding,Profile Extrusion,Extrusion