General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.14 g/cm³ Show Supplier Material materials with Density of 1.14 g/cm³ | ASTM D792 |
Water absorption, equilibrium | 23.0 °C | 0.3 % Show Supplier Material materials with Water absorption, equilibrium of 0.3 % | max., ASTM D4442 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 40 % Show Supplier Material materials with Elongation of 40 % | min., ASTM D638 |
Flexural modulus | 23.0 °C | 2.5 GPa Show Supplier Material materials with Flexural modulus of 2.5 GPa | ASTM D790 |
Flexural strength | 23.0 °C | 115 MPa Show Supplier Material materials with Flexural strength of 115 MPa | ASTM D790 |
Hardness, Shore D | 23.0 °C | 78 [-] Show Supplier Material materials with Hardness, Shore D of 78 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | 23.0 °C | 60 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 60 J/m | ASTM D256 |
Tensile strength | 23.0 °C | 67 MPa Show Supplier Material materials with Tensile strength of 67 MPa | ASTM D638 |
Thermal
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 30 g/10min Show Supplier Material materials with Melt mass-flow rate of 30 g/10min | min., ASTM D1238 | |
Shrinkage | 23.0 °C | 1.2 - 1.6 % Show Supplier Material materials with Shrinkage of 1.2 - 1.6 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Baby Strollers, Electrical and electronic parts, Information technology equipment parts, Tool housing, Sports equipment, Gear, Automobiles parts. | |
Color | Translucent |