General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.07 g/cm³ Show Supplier Material materials with Density of 1.07 g/cm³ | ASTM D792 |
Water absorption, equilibrium | 23.0 °C | 0.3 % Show Supplier Material materials with Water absorption, equilibrium of 0.3 % | max., ASTM D4442 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 80 % Show Supplier Material materials with Elongation of 80 % | min., ASTM D638 |
Flexural modulus | 23.0 °C | 1.67 GPa Show Supplier Material materials with Flexural modulus of 1.67 GPa | ASTM D790 |
Flexural strength | 23.0 °C | 70 MPa Show Supplier Material materials with Flexural strength of 70 MPa | ASTM D790 |
Hardness, Shore D | 23.0 °C | 72 [-] Show Supplier Material materials with Hardness, Shore D of 72 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | -30.0 °C | 200 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 200 J/m | min., ASTM D256 |
23.0 °C | 850 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 850 J/m | min., ASTM D256 | |
Tensile strength | 23.0 °C | 43 MPa Show Supplier Material materials with Tensile strength of 43 MPa | ASTM D638 |
Thermal
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 50 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 50 °C | ASTM D648 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Skate bracket, Baby stroller accessories, Sports equipment. | |
Color | Black |