General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.33 g/cm³ Show Supplier Material materials with Density of 1.33 g/cm³ | ASTM D792 |
Water absorption, equilibrium | 23.0 °C | 0.3 % Show Supplier Material materials with Water absorption, equilibrium of 0.3 % | max., ASTM D4442 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 5 % Show Supplier Material materials with Elongation of 5 % | max., ASTM D638 |
Flexural modulus | 23.0 °C | 6.86 GPa Show Supplier Material materials with Flexural modulus of 6.86 GPa | ASTM D790 |
Flexural strength | 23.0 °C | 205 MPa Show Supplier Material materials with Flexural strength of 205 MPa | ASTM D790 |
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Supplier Material materials with Hardness, Rockwell R of 120 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 160 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 160 J/m | ASTM D256 |
Tensile strength | 23.0 °C | 130 MPa Show Supplier Material materials with Tensile strength of 130 MPa | ASTM D638 |
Thermal
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.3 - 0.8 % Show Supplier Material materials with Shrinkage of 0.3 - 0.8 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Automobiles-Rearview mirror Rotation Axes, Medical Equipment-Wheelchair Fork | |
Color | Black | |
Fillers | 30% Glass Fiber |