General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.06 g/cm³ Show Supplier Material materials with Density of 1.06 g/cm³ | ASTM D792 |
Water absorption, equilibrium | 23.0 °C | 0.3 % Show Supplier Material materials with Water absorption, equilibrium of 0.3 % | max., ASTM D4442 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 70 % Show Supplier Material materials with Elongation of 70 % | min., ASTM D638 |
Flexural modulus | 23.0 °C | 1.81 GPa Show Supplier Material materials with Flexural modulus of 1.81 GPa | ASTM D790 |
Flexural strength | 23.0 °C | 75 MPa Show Supplier Material materials with Flexural strength of 75 MPa | ASTM D790 |
Hardness, Shore D | 23.0 °C | 76 [-] Show Supplier Material materials with Hardness, Shore D of 76 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | 23.0 °C | 700 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 700 J/m | ASTM D256 |
Tensile strength | 23.0 °C | 45 MPa Show Supplier Material materials with Tensile strength of 45 MPa | ASTM D638 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 1.6 - 2 % Show Supplier Material materials with Shrinkage of 1.6 - 2 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Sports equipment, Buckle | |
Color | Natural |