Dimension

PropertyValue

Dimensions

Round-Bar length: 16-50 mm

Chemical properties

PropertyValueComment

Carbon

0.03 %

Show Supplier Material materials with Carbon of 0.03 %

max.

Chromium

21.5 - 24.5 %

Show Supplier Material materials with Chromium of 21.5 - 24.5 %

Manganese

4.5 - 6.5 %

Show Supplier Material materials with Manganese of 4.5 - 6.5 %

Molybdenum

2.8 - 3.4 %

Show Supplier Material materials with Molybdenum of 2.8 - 3.4 %

Nickel

15.5 - 18.0 %

Show Supplier Material materials with Nickel of 15.5 - 18.0 %

Niobium

0.1 - 0.3 %

Show Supplier Material materials with Niobium of 0.1 - 0.3 %

Nitrogen

0.3 - 0.5 %

Show Supplier Material materials with Nitrogen of 0.3 - 0.5 %

Phosphorus

0.025 %

Show Supplier Material materials with Phosphorus of 0.025 %

max.

Silicon

1 %

Show Supplier Material materials with Silicon of 1 %

max.

Sulfur

0.01 %

Show Supplier Material materials with Sulfur of 0.01 %

max.

Technological properties

Property
Application areas

Shipbuilding, electrical engineering, mechanical engineering

Corrosion properties

Resistant to intercrystalline corrosion, pitting and stress corrosion

Processing history

Solution Annealed