PropertyValue

Dimensions

Round-Bar length: 20 mm

Mechanical

PropertyValueComment

Tensile strength

730 MPa

Show Supplier Material materials with Tensile strength of 730 MPa

max.

Chemical properties

PropertyValueComment

Carbon

0.08 - 0.15 %

Show Supplier Material materials with Carbon of 0.08 - 0.15 %

Chromium

12.0 - 14.0 %

Show Supplier Material materials with Chromium of 12.0 - 14.0 %

Molybdenum

0.6 %

Show Supplier Material materials with Molybdenum of 0.6 %

max.

Sulfur

0.15 - 0.35 %

Show Supplier Material materials with Sulfur of 0.15 - 0.35 %

Technological properties

Property
Application areas

Plant construction, mechanical engineering, structural parts in water and steam for automatic machining, such as screws, nuts, bolts and similar parts

Processing history

Annealed