AMS 4616

.XLSX
.PDF
Save

Description

AMS 4616 is a special high strength silicon bronze. The iron content adds strength, combined with the self lubricating properties of silicon, provides excellent bearing and load properties.

Equivalent Materials

Properties

General

Density ρ

8.5 g/cm³ at 20 °C

Mechanical

Hardness, Rockwell C HRC

55 [-] at 20 °C

Thermal

Melting point Tm

971 - 1027 °C

Chemical properties

Element

Weight %

Comment

Cu

-

Balance

Si

2.4 - 4 %

Fe

1 - 2 %

Mn

1 %

Zn

1 - 1.5 %

This material data has been provided by Righton Blackburns.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.