Mechanical

Tensile strength Rm

515 MPa at 20 °C

Yield strength YS

205 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

-

Balance

Cr

18 - 20 %

Ni

11 - 15 %

Mo

3 - 4 %

Mn

2 %

More