Description

Grade 410 / 1.4006 is a hardenable martensitic stainless steel available in bar form only.

Related Standards

Equivalent Materials

Properties

Electrical

Electrical resistivity ρel

5.7E-8 Ω·m at 20 °C

General

Density ρ

7.75 g/cm³ at 20 °C

Mechanical

Elastic modulus E

200 GPa at 20 °C

Tensile strength Rm

650 - 850 MPa at 20 °C

Yield strength YS

450 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

9.9E-6 1/K at 20 °C

Thermal conductivity λ

24.9 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

-

Balance

Cr

11.5 - 13.5 %

Mn

1.5 %

Si

1 %

Ni

0.75 %

More

Technological properties

Corrosion properties

Moderate in non-chloride containing environments

This material data has been provided by Righton Blackburns.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.