Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant and also halogen free according VDE/DIN 472 part 815. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).

Ashby charts

See where EXTEM™ Resin VH1003 - Americas falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

1.3 g/cm³ at 23 °C

ISO 1183

Limiting oxygen index

LOI

45 % at 23 °C

Moisture absorption

cmoisture

0.6 % at 23 °C

ISO 62 | (23°C / 50% RH)

Relative density

ρrel

1.3 [-] at 23 °C

ASTM D 792 |

Water absorption

cwater

1.75 % at 23 °C

ISO 62-1 | (23°C/saturated)

Mechanical

Elastic modulus

E

3.11 GPa at 23 °C

Show Polyimide (PI) materials with Elastic modulus of 3.11 GPa at 23 °C

ISO 527 | 1 mm/min

Elongation

A

8.5 % at 23 °C

Show Polyimide (PI) materials with Elongation of 8.5 % at 23 °C

ISO 527 | yield, 5 mm/min

Flexural modulus

Ebend

3.08 GPa at 23 °C

Show Polyimide (PI) materials with Flexural modulus of 3.08 GPa at 23 °C

ISO 178 | 2 mm/min

Flexural strength

σbend

123 MPa at 23 °C

Show Polyimide (PI) materials with Flexural strength of 123 MPa at 23 °C

ISO 178 | yield, 2 mm/min

Hardness, Ball Indentation

HBI

140 MPa at 23 °C

Show Polyimide (PI) materials with Hardness, Ball Indentation of 140 MPa at 23 °C

ISO 2039-1 | H358/30

Impact strength, Charpy unnotched Iunnot

ISO 179/1eU | Unnotch Edgew 80*10*4 sp=62mm, -30°C

Impact strength, Izod notched

IIzod,not

4 kJ/m² at 23 °C

Show Polyimide (PI) materials with Impact strength, Izod notched of 4 kJ/m² at 23 °C

ISO 180/1A | notched 80*10*4, 23°C

Impact strength, Izod notched, ASTM

IIzod,not,astm

69 J/m at 23 °C

Show Polyimide (PI) materials with Impact strength, Izod notched, ASTM of 69 J/m at 23 °C

ASTM D 256

Impact strength, Izod unnotched IIzod,unnot

ISO 180/1U | unnotched 80*10*4, -30°C

Impact strength, Izod unnotched, ASTM IIzod,unnot,astm

ASTM D 4812 | 23°C

Instrumented Impact, Total Energy

ItotalE

33 J at 23 °C

Show Polyimide (PI) materials with Instrumented Impact, Total Energy of 33 J at 23 °C

ASTM D 3763 | 23°C

Tensile strength

Rm

95 MPa at 23 °C

Show Polyimide (PI) materials with Tensile strength of 95 MPa at 23 °C

ISO 527 | yield, 5 mm/min

Thermal

Ball Pressure Test

Passes

Coefficient of thermal expansion

α

5E-5 1/K at 23 °C

ISO 11359-2 | 23°C to 150°C

Coefficient of thermal expansion, transverse

αtrans

5E-5 1/K at 23 °C

ISO 11359-2 | 23°C to 150°C

Flammability

Glow Wire Flammability Index 960°C, passes at: 3.2 mm IEC 60695-2-12 | Glow Wire Flammability Index 960°C, passes at: 3.2 mm IEC 60695-2-12 | UL Recognized, 94V-0 Flame Class Rating: 0.75 mm UL 94 | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=257957

Glow Wire Ignition Temperature

GWIT

850 °C

IEC 60695-2-13 | 3.0 mm

Heat deflection temperature, 0.45 MPa

HDT0.45,MPa

237 °C

ASTM D 648 | 6.4 mm, unannealed

Heat deflection temperature, 1.80 MPa

HDT1.8,MPa

228 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Relative temperature index, electrical

RTIel

160 °C

UL 746B

Relative temperature index, mechanical impact

RTIimp

120 °C

UL 746B

Relative temperature index, mechanical strength

RTIstr

160 °C

UL 746B

Thermal conductivity

λ

0.22 W/(m·K) at 23 °C

ASTM E 1530 |

Vicat softening temperature

Tsoft

238 °C

ISO 306 | Rate B/120

Electrical

Comparative tracking index

CTI

3 V at 23 °C

UL 746A | (UL) {PLC}

Dielectric constant, 100Hz

εr,100Hz

3.41 [-] at 23 °C

ASTM D 150

Dielectric strength

EDS

17 kV/mm at 23 °C

ASTM D 149 | in oil, 3.2 mm

Dissipation factor, 100Hz

ε''100Hz

8E-3 [-] at 23 °C

IEC 60250

Dissipation factor, 1MHz

ε''1MHz

7E-3 [-] at 23 °C

IEC 60250

Dissipation factor, 1kHz

ε''1KHz

1E-3 [-] at 23 °C

IEC 60250

Dissipation factor, 50Hz

ε''50Hz

0.03 [-] at 23 °C

IEC 60250 | 50/60 Hz

High Amp Arc Ignition

HAI

0.75 mm at 23 °C

UL 746A | PLC 4

Hot-Wire Ignition

HWI

3 mm at 23 °C

UL 746A | PLC 1

Optical

Haze

H

2 %

ASTM D 1003 | 2.54 mm

Transmission

t

58 %

ASTM D 1003 | 2.54 mm

Rheological Properties

Melt mass-flow rate

MFR

15.5 g/10min

ASTM D 1238 | 367°C/6.6 kgf

Melt volume-flow rate

MVR

8 cm³/10min

ISO 1133 | MVR at 360°C/5.0 kg

Shrinkage

cshrink

0.5 % at 23 °C

SABIC method | on tensile bar

Shrinkage, transverse

cshrink, trans

0.5 % at 23 °C

SABIC method | 3.2 mm

Technological properties

Application areas

Electronic Components, Personal Computing, Meter Gas

Availability

Europe,Asia,Americas

Features

High Heat Resistance

Filler Type

Processing Tag

Processing methods

Melt Temperature: 380 to 405.0 °C | Vent Depth: 0.025 to 0.076 mm | Drying Temperature: 150 °C | Maximum Moisture Content: 0.02 % | Shot to Cylinder Size: 40 to 60.0 % | Mold Temperature: 140 to 180.0 °C | Nozzle Temperature: 375 to 400.0 °C | Rear - Zone 1 Temperature: 360 to 380.0 °C | Drying Time: 4 to 6.0 hrs | Front - Zone 3 Temperature: 380 to 405.0 °C | Middle - Zone 2 Temperature: 370 to 395.0 °C | Drying Time (Cumulative): 24 hrs | Back pressure (Plastic Pressure): 5 to 10.0 MPa | Screw speed (Circumferential speed): 0.2 m/s | Intake (throat) temperature: 70 to 100.0 °C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.