LEXAN FXD123R is a transparent/translucent low viscosity grade for light diffusion special effects. UV-stabilized. Color package may affect performance.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Water absorption

23.0 °C

0.35 %

Show Supplier Material materials with Water absorption of 0.35 %

ISO 62-1 | (23°C/saturated)

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

220 %

Show Supplier Material materials with Elongation of 220 %

SABIC - Japan Method | break

Flexural modulus

23.0 °C

2.3 GPa

Show Supplier Material materials with Flexural modulus of 2.3 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

90 MPa

Show Supplier Material materials with Flexural strength of 90 MPa

ISO 178 | yield, 2 mm/min

Impact strength, Izod notched

23.0 °C

65 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 65 kJ/m²

ISO 180/1A | 80*10*3, 23°C

Tensile strength

23.0 °C

61 MPa

Show Supplier Material materials with Tensile strength of 61 MPa

SABIC - Japan Method | yield

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

7E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 7E-5 1/K

TMA | -30°C to 30°C

Heat deflection temperature, 0.45 MPa

133 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 133 °C

ISO 75/Be | Edgew 120*10*4 sp=100mm

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

SABIC method | on tensile bar

Technological properties

Property
Application areas

Audio, Auto Aftermarket, Data Transfer, Data Management, Cluster, Console, Displays, Doors Hardware/Trim, Forward Lighting, Heavy Vehicles, Infotainment/Telematic, Electronic Components, Power Manangement, Rear/Signal Lighting, Small Appliance, Surgical Devices, Non-LED Lighting, Personal Computing, Meter Gas, LED Lighting, Wireless Communications, Trim

Availability

Europe,Asia

Features

UV Resistant, Aesthetics & Visual effects

Processing methods

Front

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.