SILTEM™ resin STM1600 - Americas

Want to keep this datasheet? Save it now in your required format

Description

SILTEM™ STM1600 resin is a flexible polyetherimide(PEI)-siloxane copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity. It is an amber colored transparent material that can be selfcolored and easily processed on conventional equipment. The material may also have a fit in flexible profiles or injection molded parts.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.19 g/cm³

Show Supplier Material materials with Density of 1.19 g/cm³

ISO 1183

Limiting oxygen index

23.0 °C

48 %

Show Supplier Material materials with Limiting oxygen index of 48 %

Relative density

23.0 °C

1.19 [-]

Show Supplier Material materials with Relative density of 1.19 [-]

ASTM D 792

Water absorption

23.0 °C

0.58 %

Show Supplier Material materials with Water absorption of 0.58 %

ISO 62-1 | (23°C/saturated)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.38 GPa

Show Supplier Material materials with Elastic modulus of 1.38 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

10 %

Show Supplier Material materials with Elongation of 10 %

ISO 527 | yield, 50 mm/min

Flexural modulus

23.0 °C

1.25 GPa

Show Supplier Material materials with Flexural modulus of 1.25 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

55 MPa

Show Supplier Material materials with Flexural strength of 55 MPa

ISO 178 | yield, 2 mm/min

Hardness, Shore D

23.0 °C

72 [-]

Show Supplier Material materials with Hardness, Shore D of 72 [-]

ASTM D 2240

Impact strength, Izod notched

23.0 °C

25 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 25 kJ/m²

ISO 180/1A | notched 80*10*4, -30°C

Taber Abrasion

23.0 °C

50 mg/1000cy

Show Supplier Material materials with Taber Abrasion of 50 mg/1000cy

ASTM D 1044 | CS-17, 1 kg

Tensile strength

23.0 °C

41 MPa

Show Supplier Material materials with Tensile strength of 41 MPa

ISO 527 | break, 50 mm/min

Thermal

PropertyValueComment

Glass transition temperature

195 °C

Show Supplier Material materials with Glass transition temperature of 195 °C

DMA | matrix

Heat deflection temperature, 0.45 MPa

144 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 144 °C

ISO 75/Bf | Flatw 80*10*4 sp=64mm

Vicat softening temperature

167 °C

Show Supplier Material materials with Vicat softening temperature of 167 °C

ISO 306 | Rate B/120

Flammability

UL Compliant, 94V-0 Flame Class Rating: 1.6mm UL 94 by SABIC-IP

Electrical

PropertyTemperatureValueComment

Dielectric constant, 100Hz

23.0 °C

3.14 [-]

Show Supplier Material materials with Dielectric constant, 100Hz of 3.14 [-]

ASTM D 150

Dielectric constant, 1KHz

23.0 °C

3 [-]

Show Supplier Material materials with Dielectric constant, 1KHz of 3 [-]

ASTM D 150

Dielectric constant, 1MHz

23.0 °C

3.02 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 3.02 [-]

ASTM D 150

Dielectric strength

23.0 °C

16.6 kV/mm

Show Supplier Material materials with Dielectric strength of 16.6 kV/mm

ASTM D 149 | in oil, 3.2 mm

Dissipation factor, 100Hz

23.0 °C

0.01 [-]

Show Supplier Material materials with Dissipation factor, 100Hz of 0.01 [-]

ASTM D 150

Dissipation factor, 100kHz

23.0 °C

6.4E-3 [-]

Show Supplier Material materials with Dissipation factor, 100kHz of 6.4E-3 [-]

ASTM D 150

Dissipation factor, 1MHz

23.0 °C

5.5E-3 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 5.5E-3 [-]

ASTM D 150

Sheet resistivity, ROA

23.0 °C

1.00E+15 Ω

Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω

>, ASTM D 257

Volume resistivity

23.0 °C

1.00E+16 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm

>, ASTM D 257

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

8.6 g/10min

Show Supplier Material materials with Melt mass-flow rate of 8.6 g/10min

ASTM D 1238 | 295°C/6.6 kgf

Shrinkage

23.0 °C

0.86 %

Show Supplier Material materials with Shrinkage of 0.86 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Fluid Delivery, Enclosure/Housing/Cover, Aerospace, Wire & cable

Availability

Europe,Americas

Features

Low Corrosivity, High Tensile Elongation, Flexible, Chemical Resistance, Low Smoke and Toxicity, High Heat Resistance, Good dimensional stability, Flame Retardant, Non-Halogenated

Processing methods

Drying Temperature: 110 to 130.0°C
Feed Zone Temperature: 270 to 310.0°C
Drying Time: 4 to 6.0hrs
Back Pressure: 0.3 to 0.7MPa
Drying Time (Cumulative): 8hrs
Screw Speed: 5 to 50.0rpm
Cross-head Temperature: 290 to 330.0°C
Rear - Zone 1 Temperature: 310 to 320.0°C
Screw Speed: 50 to 100.0rpm
Die Temperature: 290 to 330.0°C
Melt Temperature: 290 to 330.0°C
Middle - Zone 2 Temperature: 310 to 320.0°C
Melt Temperature: 310 to 320.0°C
Shot to Cylinder Size: 40 to 60.0%
Screen Pack: 100 to 200.0-
Nozzle Temperature: 310 to 320.0°C
Front - Zone 3 Temperature: 310 to 320.0°C
Mold Temperature: 105 to 115.0°C
Conductor Pre-heat Temperature: 100 to 150.0°C
Drying Time: 5 to 7.0hrs
Middle Zone Temperatures: 280 to 320.0°C
Head Zone Temperature: 290 to 330.0°C
Maximum Moisture Content: 0.02%
Drying Temperature: 105°C
Water Bath Temperature: 70 to 90.0°C
Maximum Moisture Content: 0.02%
Neck Temperature: 290 to 330.0°C
Vent Depth: 0.025 to 0.076mm
Extruder Length/Diameter Ratio (L/D): 22:1 to 28:1-
Compression Ratio: 2.1:1 to 2.7:1-

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.