NORYL™ Resin CRX1005 - Europe

Want to keep this datasheet? Save it now in your required format

Description

NORYL™ CRX1005 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable and extrusion grade was developed with improved chemical resistance and exhibits low moisture absorption, creep resistance, dimensional stability, and hydrolytic stability.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

150 %

Show Supplier Material materials with Elongation of 150 %

SABIC - Japan Method | break

Flexural modulus

23.0 °C

1.8 GPa

Show Supplier Material materials with Flexural modulus of 1.8 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

55 MPa

Show Supplier Material materials with Flexural strength of 55 MPa

ISO 178 | yield, 2 mm/min

Impact strength, Izod notched

23.0 °C

21 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 21 kJ/m²

ISO 180/1A | notched 80*10*4, 23°C

Tensile strength

23.0 °C

35 MPa

Show Supplier Material materials with Tensile strength of 35 MPa

SABIC - Japan Method | yield

Thermal

PropertyValueComment

Heat deflection temperature

95 °C

Show Supplier Material materials with Heat deflection temperature of 95 °C

Heat deflection temperature, 1.80 MPa

95 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 95 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Technological properties

Property
Application areas

Vacuum Cleaner, Washing Machine, Pipe/Fitting, Plumbing, Hot Water System

Availability

Asia

Features

Hydrolytic Stability, Low Creep Sensitivity, High Impact Resistance

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.