ULTEM R16SG00 sheet is an extruded Polyetherimide (PEI) alloy sheet material used for rail interior applications. ULTEM R16SG00 sheet is an amorphous thermoplastic offering outstanding high heat resistance, high strength, modulus and broad chemical resistance. ULTEM R16SG00 sheet is inherently flame resistant with low smoke emission. ULTEM R16SG00 sheet meets United States Federal Rail Administration (FRA 49 CFR Part 238, Appendix B) flammability and smoke emission characteristics for passenger cars and locomotive cabs. The material may be thermoformed, pressure formed, twin sheet formed, or used in flat or cold formed applications. Information on stain and chemical resistance, processing, and secondary operations is available upon request.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.27 g/cm³

Show Supplier Material materials with Density of 1.27 g/cm³

ISO 1183

Technological properties

Property
Availability

Europe,Asia,MEA,Americas,Global

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.