OF-Cu Copper

.XLSX
.PDF
Save

Description

Oxygen free copper grade

Equivalent Materials

Properties

General

Density ρ

8.9 g/cm³ at 20 °C

Mechanical

Elastic modulus E

127 GPa at 20 °C

Elongation A

5 - 45 % at 20 °C

hard - soft

Hardness, Brinell HB

45 - 95 [-] at 20 °C

Tensile strength Rm

215 - 375 MPa at 20 °C

Yield strength YS

50 - 320 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.77E-5 1/K at 20 °C

Thermal conductivity λ

393 W/(m·K) at 20 °C

Electrical

Electrical conductivity σel

5.80E+7 S/m at 20 °C

This material data has been provided by Salomons Metalen.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.