CuCo2Be Cobalt Beryllium Copper

.XLSX
.PDF
Save

Description

Alloyed copper grade

Equivalent Materials

Properties

Electrical

Electrical conductivity σel

2.50E+7 S/m at 20 °C

General

Density ρ

8.8 g/cm³ at 20 °C

Mechanical

Elastic modulus E

135 GPa at 20 °C

Elongation A

1 - 20 % at 20 °C

hard - soft

Hardness, Brinell HB

180 - 260 [-] at 20 °C

Tensile strength Rm

650 - 1000 MPa at 20 °C

Yield strength YS

500 - 980 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.8E-5 1/K at 20 °C

Thermal conductivity λ

239 W/(m·K) at 20 °C

This material data has been provided by Salomons Metalen.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.