CuZn30 Brass

.XLSX
.PDF
Save

Description

Cartridge Brass

Equivalent Materials

Properties

General

Density ρ

8.5 g/cm³ at 20 °C

Mechanical

Elastic modulus E

114 GPa at 20 °C

Elongation A

8 - 50 % at 20 °C

hard - soft

Hardness, Brinell HB

55 - 150 [-] at 20 °C

Tensile strength Rm

270 - 520 MPa at 20 °C

Yield strength YS

160 - 470 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.97E-5 1/K at 20 °C

Thermal conductivity λ

126 W/(m·K) at 20 °C

Electrical

Electrical conductivity σel

1.63E+7 S/m at 20 °C