AI99.5 - F7 condition

Alternative and trade names
1S
Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by Salomons Metalen.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.7 g/cm³

Show Supplier Material materials with Density of 2.7 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

69 GPa

Show Supplier Material materials with Elastic modulus of 69 GPa

Elongation A5

23.0 °C

25 %

Show Supplier Material materials with Elongation A5 of 25 %

Hardness, Brinell

23.0 °C

20 [-]

Show Supplier Material materials with Hardness, Brinell of 20 [-]

Tensile strength

23.0 °C

65 MPa

Show Supplier Material materials with Tensile strength of 65 MPa

Yield strength Rp0.2

23.0 °C

20 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 20 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

2.35E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.35E-5 1/K

Thermal conductivity

23.0 °C

220 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 220 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

3.50E+7 S/m

Show Supplier Material materials with Electrical conductivity of 3.50E+7 S/m

Chemical properties

PropertyValue

Aluminium

99.5 %

Show Supplier Material materials with Aluminium of 99.5 %

Copper

0.05 %

Show Supplier Material materials with Copper of 0.05 %

Iron

0.4 %

Show Supplier Material materials with Iron of 0.4 %

Magnesium

0.05 %

Show Supplier Material materials with Magnesium of 0.05 %

Manganese

0.05 %

Show Supplier Material materials with Manganese of 0.05 %

Other

0.03 %

Show Supplier Material materials with Other of 0.03 %

Silicon

0.25 %

Show Supplier Material materials with Silicon of 0.25 %

Titanium

0.05 %

Show Supplier Material materials with Titanium of 0.05 %

Zinc

0.07 %

Show Supplier Material materials with Zinc of 0.07 %