Stainless Steel 631 (17-7PH)

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by Salomons Metalen.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValueComment

Aluminium

0.75 - 1.5 %

Show Supplier Material materials with Aluminium of 0.75 - 1.5 %

Carbon

0.09 %

Show Supplier Material materials with Carbon of 0.09 %

Chromium

16 - 18 %

Show Supplier Material materials with Chromium of 16 - 18 %

Iron

70.58 - 76.75 %

Show Supplier Material materials with Iron of 70.58 - 76.75 %

Balance

Manganese

1 %

Show Supplier Material materials with Manganese of 1 %

Nickel

6.5 - 7.75 %

Show Supplier Material materials with Nickel of 6.5 - 7.75 %

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

Silicon

1 %

Show Supplier Material materials with Silicon of 1 %

Sulfur

0.03 %

Show Supplier Material materials with Sulfur of 0.03 %