Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A5 | 23.0 °C | 10 - 18 % Show Supplier Material materials with Elongation A5 of 10 - 18 % |
Hardness, Brinell | 23.0 °C | 370 [-] Show Supplier Material materials with Hardness, Brinell of 370 [-] |
Tensile strength | 23.0 °C | 900 - 990 MPa Show Supplier Material materials with Tensile strength of 900 - 990 MPa |
Yield strength Rp0.2 | 23.0 °C | 830 MPa Show Supplier Material materials with Yield strength Rp0.2 of 830 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 5.5 - 6.7 % Show Supplier Material materials with Aluminium of 5.5 - 6.7 % |
Titanium | Balance |
Vanadium | 3.5 - 4.5 % Show Supplier Material materials with Vanadium of 3.5 - 4.5 % |