General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.4 g/cm³ Show Supplier Material materials with Density of 1.4 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 25 % Show Supplier Material materials with Elongation of 25 % | ISO 527 |
Flexural modulus | 23.0 °C | 3.2 GPa Show Supplier Material materials with Flexural modulus of 3.2 GPa | ISO 178 |
Flexural strength | 23.0 °C | 100 MPa Show Supplier Material materials with Flexural strength of 100 MPa | ISO 178 |
Impact strength, Charpy notched | 23.0 °C | 7.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 7.5 kJ/m² | ISO 179 |
Tensile strength | 23.0 °C | 80 MPa Show Supplier Material materials with Tensile strength of 80 MPa | ISO 527 |
Thermal
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 150 V Show Supplier Material materials with Comparative tracking index of 150 V | IEC 60112 |
Dielectric constant | 23.0 °C | 2.8 [-] Show Supplier Material materials with Dielectric constant of 2.8 [-] | IEC 60250 |
Dielectric strength | 23.0 °C | 26 kV/mm Show Supplier Material materials with Dielectric strength of 26 kV/mm | IEC 60243 |
Dissipation factor | 23.0 °C | 4E-3 [-] Show Supplier Material materials with Dissipation factor of 4E-3 [-] | IEC 60250 |
Volume resistivity | 23.0 °C | 1.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm | IEC 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical pump pump body and impeller, cable plug, junction box, ultra pure water system pipe fittings and valves.Engine bearing, shim, sealing element, clutch ring.The driving and brake parts of a car. Cable, wire, coil skeleton, connector, etc | |
Processing methods | Extrusion or Injection Moulding / Test Specimen Production: Drying 150°C & 3 hours/120°C & 5 hours - Injection molding melt temperature: 355-375°C - Injection molding mold temperature: 170-200°C |