PEEK CF30 G PTFE SGC301E43

Alternative and trade names
EK-SGC301E43
Want to keep this datasheet? Save it now in your required format

Description

It is a 30% CF, PTFE and graphite reinforced PEEK compound developed to provide excellent wear resistance, lower coefficient of friction and better chemical resistant.

This material data has been provided by Sciengy New Materials Co. Ltd.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.45 g/cm³

Show Supplier Material materials with Density of 1.45 g/cm³

ISO 1183

Water absorption

23.0 °C

0.04 %

Show Supplier Material materials with Water absorption of 0.04 %

ISO 62

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

2.2 %

Show Supplier Material materials with Elongation of 2.2 %

ISO 527

Flexural modulus

23.0 °C

11 GPa

Show Supplier Material materials with Flexural modulus of 11 GPa

ISO 178

Flexural strength

23.0 °C

230 MPa

Show Supplier Material materials with Flexural strength of 230 MPa

ISO 178

Impact strength, Charpy notched

23.0 °C

8 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 8 kJ/m²

ISO 179

Tensile strength

23.0 °C

150 MPa

Show Supplier Material materials with Tensile strength of 150 MPa

ISO 527

Thermal

PropertyTemperatureValueComment

Heat deflection temperature, 1.80 MPa

315 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 315 °C

ISO 75

Melting point

343 °C

Show Supplier Material materials with Melting point of 343 °C

ISO 11357 (10°C/min)

Thermal conductivity

23.0 °C

0.8 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 0.8 W/(m·K)

ISO 22007-4

Flammability

V-0, UL-94

Electrical

PropertyTemperatureValueComment

Volume resistivity

23.0 °C

1.00E+10 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+10 Ω·cm

IEC 60093

Technological properties

Property
Application areas

Chemical pump pump body and impeller, cable plug, junction box, ultra pure water system pipe fittings and valves.Engine bearing, shim, sealing element, clutch ring.The driving and brake parts of a car. Cable, wire, coil skeleton, connector, etc

Fillers

30% Carbon Fiber and PTFE

Processing methods

Extrusion or Injection Moulding / Test Specimen Production: Drying 150°C & 3 hours/120°C & 5 hours - Injection molding melt temperature: 360-385°C - Injection molding mold temperature: 180-200°C