With a high alkali and alkaline earth oxide content and a general sealing glass with high chemical resistance.

This material data has been provided by Schott Glass Tubing.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.5 g/cm³

Show Supplier Material materials with Density of 2.5 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

73 GPa

Show Supplier Material materials with Elastic modulus of 73 GPa

Poisson's ratio

23.0 °C

0.22 [-]

Show Supplier Material materials with Poisson's ratio of 0.22 [-]

Thermal

PropertyTemperatureValueComment

Annealing temperature

530 °C

Show Supplier Material materials with Annealing temperature of 530 °C

Viscosity 10¹³ dPa.s (ISO 7884-4)

Coefficient of thermal expansion

23.0 °C

9.1E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 9.1E-6 1/K

mean value for 20-300 °C - ISO 7991

Glass transition temperature

525 °C

Show Supplier Material materials with Glass transition temperature of 525 °C

ISO 7884-8

Softening temperature

720 °C

Show Supplier Material materials with Softening temperature of 720 °C

Viscosity 10⁷·⁶ dPa.s (ISO 7884-3)

Specific electrical resistance temperature

200 °C

Show Supplier Material materials with Specific electrical resistance temperature of 200 °C

For ρ = 10⁸ Ω·cm

Thermal conductivity

90.0 °C

1.1 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 1.1 W/(m·K)

Working temperature

1040 °C

Show Supplier Material materials with Working temperature of 1040 °C

Viscosity 10⁴ dPa.s (ISO 7884-2)

Electrical

PropertyTemperatureValue

Dielectric constant, 1MHz

23.0 °C

7.2 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 7.2 [-]

Electrical resistivity

250.0 °C

125892 Ω·m

Show Supplier Material materials with Electrical resistivity of 125892 Ω·m

350.0 °C

5011 Ω·m

Show Supplier Material materials with Electrical resistivity of 5011 Ω·m

Loss tangent, 1MHz

23.0 °C

7E-3 [-]

Show Supplier Material materials with Loss tangent, 1MHz of 7E-3 [-]

Optical

PropertyValueComment

Refractive index

1.51 [-]

Show Supplier Material materials with Refractive index of 1.51 [-]

at λ=587.6 nm

Stress optical coefficient

2.7E-6 mm²/N

Show Supplier Material materials with Stress optical coefficient of 2.7E-6 mm²/N

DIN 52314

Chemical properties

PropertyValueComment

Aluminium

4 %

Show Supplier Material materials with Aluminium of 4 %

Al₂O₃

Barium

2 %

Show Supplier Material materials with Barium of 2 %

BaO

Boron

1 %

Show Supplier Material materials with Boron of 1 %

B₂O₃

Calcium

5 %

Show Supplier Material materials with Calcium of 5 %

CaO

Magnesium

3 %

Show Supplier Material materials with Magnesium of 3 %

MgO

Other

0.01 %

Show Supplier Material materials with Other of 0.01 %

max., Lead, Cadmium, Mercury and Hexavalent Chromium

Potassium

3 %

Show Supplier Material materials with Potassium of 3 %

K₂O

Silicon

69 %

Show Supplier Material materials with Silicon of 69 %

SiO₂

Sodium

13 %

Show Supplier Material materials with Sodium of 13 %

Na₂O

Technological properties

Property
Application areas

Engineering (Heat exchanger, Glass apparatus, Instrument / Barometers / Aerometers / Sightglasses and Others), Renewable energy (Photovoltaics, Solar collectors, Receiver), Signal intensifier, Detector and (fibre-) optics (Transmitter and x-ray tubes, other Fibre optics, other Electrotechnology/Electronics), Home (Glass fibre applications, Aquarium heating tubes, Furniture, Sprinkler fuses, Food packaging /cosmetics, Architecture, Christmas Ornaments, Giftware and others), Lighting (Explosion roof lighting, Neon tubing, Lamp bulbs, Exhaust and plate tubing and others), Laboratory/Industrial Technology (Glassblown laboratory ware, Test tubes, Measuring cylinders, Pressed glass articles like balls and lenses, Medical technology like microlitetre syringe and pipettes, Thermometry), Pharmaceutical packaging (Vials, Tablet bottles), Glass straws.

Corrosion properties

Hydrolytic resistance Class HGB3 (ISO 719), Type III (Ph. Eur.), Type III (USP) - Acid resistance Class S1 (DIN 12116) - Alkali resistance Class A2 (ISO695), ASTM E 438 Type II