CONTURAX® Pro

Alternative and trade names
CONTURAX® Pro
.XLSX
.PDF
Save

Description

Acc. to ISO 3585. It exhibits high chemical resistance, high hydrolytic resistance and high resistance to thermal shock.

Properties

General

Density ρ

2.23 g/cm³ at 20 °C

Mechanical

Elastic modulus E

63 GPa at 20 °C

Poisson's ratio ν

0.2 [-] at 20 °C

Thermal

Annealing temperature Tanneal

560 °C

Viscosity 10¹³ dPa.s (ISO 7884-4)

Coefficient of thermal expansion α

3.3E-6 1/K at 20 °C

mean value for 20-300 °C - ISO 7991

Glass transition temperature Tg

525 °C

ISO 7884-8

Softening temperature Tsoftening

825 °C

Viscosity 10⁷·⁶ dPa.s (ISO 7884-3)

Specific electrical resistance temperature Tk

250 °C

For ρ = 10⁸ Ω·cm

Thermal conductivity λ

1.2 W/(m·K) at 90 °C

Working temperature Tworking

1260 °C

Viscosity 10⁴ dPa.s (ISO 7884-2)

Electrical

Dielectric constant, 1MHz εr,1MHz

4.6 [-] at 20 °C

Electrical resistivity ρel

1000000 Ω·m at 250 °C

Show chart

Loss tangent, 1MHz tanδ1,MHz

3.7E-3 [-] at 20 °C

Optical

Refractive index nd

1.47 [-]

at λ=587.6 nm

Stress optical coefficient k

4E-6 mm²/N

DIN 52314

Chemical properties

Element

Weight %

Comment

Other

0.01 %

max., Lead, Cadmium, Mercury and Hexavalent Chromium

Technological properties

Application areas

Engineering (Glass apparatus, Instrument / Barometers / Aerometers / Sightglasses), Signal intensifier, Detector and (fibre-) optics (other Electrotechnology/Electronics), Home (Furniture, Architecture, Partition walls, Giftware and others), Lighting (Purification/germicidal UVC/UVB/UV-CCL lamps, Safety lighting) and Laboratory/Industrial Technology (Glassblown ware and technical articles), Sprinkler, Art installations

Corrosion properties

Hydrolytic resistance Class HGB1 (ISO 719) - Acid resistance Class S1 (DIN 12116) - Alkali resistance Class A2 (ISO695)

This material data has been provided by Schott Glass Tubing.