Sealing glasses in general with 33.5% PbO, electrically highly insulating and highly x-ray-absorbing.

This material data has been provided by Schott Glass Tubing.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

20.0 °C

3.28 g/cm³

Show Supplier Material materials with Density of 3.28 g/cm³

Thermal

PropertyTemperatureValueComment

Annealing temperature

465 °C

Show Supplier Material materials with Annealing temperature of 465 °C

Viscosity 10¹³ dPa.s (ISO 7884-4)

Coefficient of thermal expansion

20.0 °C

9.6E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 9.6E-6 1/K

mean value for 20-300 °C - ISO 7991

Glass transition temperature

465 °C

Show Supplier Material materials with Glass transition temperature of 465 °C

ISO 7884-8

Softening temperature

655 °C

Show Supplier Material materials with Softening temperature of 655 °C

Viscosity 10⁷·⁶ dPa.s (ISO 7884-3)

Working temperature

960 °C

Show Supplier Material materials with Working temperature of 960 °C

Viscosity 10⁴ dPa.s (ISO 7884-2)

Optical

PropertyValueComment

Refractive index

1.6 [-]

Show Supplier Material materials with Refractive index of 1.6 [-]

at λ=587.6 nm

Technological properties

Property
Application areas

TV tubes

Corrosion properties

Hydrolytic resistance Class HGB3 (ISO 719)