Borosilicate Glass SCHOTT 8229

Alternative and trade names
SCHOTT 8229
Want to keep this datasheet? Save it now in your required format

Description

Intermediate sealing glass for sealing to Glass 8228 and Glass 8230 with high resistance to thermal shock.

This material data has been provided by Schott Glass Tubing.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.17 g/cm³

Show Supplier Material materials with Density of 2.17 g/cm³

Thermal

PropertyTemperatureValueComment

Annealing temperature

637 °C

Show Supplier Material materials with Annealing temperature of 637 °C

Viscosity 10¹³ dPa.s (ISO 7884-4)

Coefficient of thermal expansion

23.0 °C

2E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2E-6 1/K

mean value for 20-300 °C - ISO 7991

Glass transition temperature

600 °C

Show Supplier Material materials with Glass transition temperature of 600 °C

ISO 7884-8

Softening temperature

930 °C

Show Supplier Material materials with Softening temperature of 930 °C

Viscosity 10⁷·⁶ dPa.s (ISO 7884-3)

Specific electrical resistance temperature

350 °C

Show Supplier Material materials with Specific electrical resistance temperature of 350 °C

For ρ = 10⁸ Ω·cm

Working temperature

1440 °C

Show Supplier Material materials with Working temperature of 1440 °C

Viscosity 10⁴ dPa.s (ISO 7884-2)

Chemical properties

PropertyValueComment

Other

0.01 %

Show Supplier Material materials with Other of 0.01 %

max., Lead, Cadmium, Mercury and Hexavalent Chromium

Technological properties

Property
Application areas

For use in electrotechnology (Signal intensifier, Detector) and lighting (Flash lights), Camera- and Video components, Digital projection, Photodynamic Therapy, Beauty and Cosmetics