Borosilicate Glass SCHOTT 8230

Alternative and trade names
SCHOTT 8230
Want to keep this datasheet? Save it now in your required format

Description

Intermediate sealing glass for sealing to Glass 8229 and Glass 8330 with high resistance to thermal shock.

This material data has been provided by Schott Glass Tubing.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

2.19 g/cm³

Show Supplier Material materials with Density of 2.19 g/cm³

Thermal

PropertyValueTesting StandardComment

Annealing temperature

590.0 °C

Show Supplier Material materials with Annealing temperature of 590.0 °C

ISO 7884-4

Viscosity 10¹³ dPa·s

Coefficient of thermal expansion

2.7e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.7e-06 1/K

ISO 7991

mean value for 20-300 °C

Glass transition temperature

570 °C

Show Supplier Material materials with Glass transition temperature of 570 °C

ISO 7884-8

Softening temperature

915.0 °C

Show Supplier Material materials with Softening temperature of 915.0 °C

ISO 7884-3

Viscosity 10⁷·⁶ dPa·s

Specific electrical resistance temperature

255.0 °C

Show Supplier Material materials with Specific electrical resistance temperature of 255.0 °C

For ρ=10⁸ Ω·cm

Working temperature

1425.0 °C

Show Supplier Material materials with Working temperature of 1425.0 °C

ISO 7884-2

Viscosity 10⁴ dPa·s

Chemical properties

Property

Other

0.01 %

max., Lead, Cadmium, Mercury and Hexavalent Chromium

Technological properties

Property
Application areas

For use in electrotechnology (Signal intensifier, Detector) and lighting (Flash lights), Camera- and Video components, Digital projection, Photodynamic Therapy, Beauty and Cosmetics