Borosilicate Glass SCHOTT 8242

Alternative and trade names
SCHOTT 8242
Want to keep this datasheet? Save it now in your required format

Description

For sealing to kovar metal and molybdenum. Electrically highly insulating.

This material data has been provided by Schott Glass Tubing.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

2.27 g/cm³

Show Supplier Material materials with Density of 2.27 g/cm³

Thermal

PropertyValueTesting StandardComment

Annealing temperature

480.0 °C

Show Supplier Material materials with Annealing temperature of 480.0 °C

ISO 7884-4

Viscosity 10¹³ dPa·s

Coefficient of thermal expansion

4.7e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 4.7e-06 1/K

ISO 7991

mean value for 20-300 °C

Glass transition temperature

465 °C

Show Supplier Material materials with Glass transition temperature of 465 °C

ISO 7884-8

Softening temperature

715.0 °C

Show Supplier Material materials with Softening temperature of 715.0 °C

ISO 7884-3

Viscosity 10⁷·⁶ dPa·s

Working temperature

1130.0 °C

Show Supplier Material materials with Working temperature of 1130.0 °C

ISO 7884-2

Viscosity 10⁴ dPa·s

Optical

PropertyValueComment

Refractive index

1.5 [-]

Show Supplier Material materials with Refractive index of 1.5 [-]

at λ=587.6 nm

Chemical properties

Property

Other

0.01 %

max., Lead, Cadmium, Mercury and Hexavalent Chromium

Technological properties

Property
Application areas

For use in clad tube for optical fibers, Endoscopy

Corrosion properties

Hydrolytic resistance Class HGB2 (ISO 719) - Acid resistance Class S4 (DIN 12116) - Alkali resistance Class A3 (ISO695)