Borosilicate Glass SCHOTT 8245

Alternative and trade names
SCHOTT 8245
Want to keep this datasheet? Save it now in your required format

Description

For sealing to kovar metal and molybdenum with minimum X-ray absorption, chemically highly resistance and electrically highly insulating.

This material data has been provided by Schott Glass Tubing.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

2.31 g/cm³

Show Supplier Material materials with Density of 2.31 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

68 GPa

Show Supplier Material materials with Elastic modulus of 68 GPa

Poisson's ratio

20.0 °C

0.22 [-]

Show Supplier Material materials with Poisson's ratio of 0.22 [-]

Thermal

PropertyTemperatureValueComment

Annealing temperature

515 °C

Show Supplier Material materials with Annealing temperature of 515 °C

Viscosity 10¹³ dPa.s (ISO 7884-4)

Coefficient of thermal expansion

20.0 °C

5.1E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 5.1E-6 1/K

mean value for 20-300 °C - ISO 7991

Glass transition temperature

505 °C

Show Supplier Material materials with Glass transition temperature of 505 °C

ISO 7884-8

Softening temperature

720 °C

Show Supplier Material materials with Softening temperature of 720 °C

Viscosity 10⁷·⁶ dPa.s (ISO 7884-3)

Specific electrical resistance temperature

215 °C

Show Supplier Material materials with Specific electrical resistance temperature of 215 °C

For ρ = 10⁸ Ω·cm

Thermal conductivity

90.0 °C

1.2 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 1.2 W/(m·K)

Working temperature

1040 °C

Show Supplier Material materials with Working temperature of 1040 °C

Viscosity 10⁴ dPa.s (ISO 7884-2)

Electrical

PropertyTemperatureValue

Dielectric constant, 1MHz

20.0 °C

5.7 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 5.7 [-]

Electrical resistivity

250.0 °C

251188 Ω·m

Show Supplier Material materials with Electrical resistivity of 251188 Ω·m

350.0 °C

7943 Ω·m

Show Supplier Material materials with Electrical resistivity of 7943 Ω·m

Loss tangent, 1MHz

20.0 °C

8E-4 [-]

Show Supplier Material materials with Loss tangent, 1MHz of 8E-4 [-]

Optical

PropertyValueComment

Refractive index

1.49 [-]

Show Supplier Material materials with Refractive index of 1.49 [-]

at λ=587.6 nm

Stress optical coefficient

3.8E-6 mm²/N

Show Supplier Material materials with Stress optical coefficient of 3.8E-6 mm²/N

DIN 52314

Chemical properties

PropertyValueComment

Other

0.01 %

Show Supplier Material materials with Other of 0.01 %

max., Lead, Cadmium, Mercury and Hexavalent Chromium

Technological properties

Property
Application areas

Signal intensifier, detector and (fibre-) optics (Transmitter, X-ray tubes, Video-frequency tubes, Photomultiplier tubes), Sensors, Lasers.

Corrosion properties

Hydrolytic resistance Class HGB3 (ISO 719) - Acid resistance Class S4 (DIN 12116) - Alkali resistance Class A3 (ISO695)