Borosilicate Glass SCHOTT 8337B

Alternative and trade names
SCHOTT 8337B
Want to keep this datasheet? Save it now in your required format

Description

For sealing to kovar metal and tungsten. Highly UV-transmitting and high resistance to thermal shock.

This material data has been provided by Schott Glass Tubing.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.22 g/cm³

Show Supplier Material materials with Density of 2.22 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

51 GPa

Show Supplier Material materials with Elastic modulus of 51 GPa

Poisson's ratio

23.0 °C

0.22 [-]

Show Supplier Material materials with Poisson's ratio of 0.22 [-]

Thermal

PropertyTemperatureValueComment

Annealing temperature

465 °C

Show Supplier Material materials with Annealing temperature of 465 °C

Viscosity 10¹³ dPa.s (ISO 7884-4)

Coefficient of thermal expansion

23.0 °C

4.1E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 4.1E-6 1/K

mean value for 20-300 °C - ISO 7991

Glass transition temperature

440 °C

Show Supplier Material materials with Glass transition temperature of 440 °C

ISO 7884-8

Softening temperature

705 °C

Show Supplier Material materials with Softening temperature of 705 °C

Viscosity 10⁷·⁶ dPa.s (ISO 7884-3)

Specific electrical resistance temperature

315 °C

Show Supplier Material materials with Specific electrical resistance temperature of 315 °C

For ρ = 10⁸ Ω·cm

Thermal conductivity

90.0 °C

1 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 1 W/(m·K)

Working temperature

1085 °C

Show Supplier Material materials with Working temperature of 1085 °C

Viscosity 10⁴ dPa.s (ISO 7884-2)

Electrical

PropertyTemperatureValue

Dielectric constant, 1MHz

23.0 °C

4.7 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 4.7 [-]

Electrical resistivity

250.0 °C

1.58E+7 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.58E+7 Ω·m

350.0 °C

316227 Ω·m

Show Supplier Material materials with Electrical resistivity of 316227 Ω·m

Loss tangent, 1MHz

23.0 °C

2.2E-3 [-]

Show Supplier Material materials with Loss tangent, 1MHz of 2.2E-3 [-]

Optical

PropertyValueComment

Refractive index

1.48 [-]

Show Supplier Material materials with Refractive index of 1.48 [-]

at λ=587.6 nm

Stress optical coefficient

4.1E-6 mm²/N

Show Supplier Material materials with Stress optical coefficient of 4.1E-6 mm²/N

DIN 52314

Chemical properties

PropertyValueComment

Other

0.01 %

Show Supplier Material materials with Other of 0.01 %

max., Lead, Cadmium, Mercury and Hexavalent Chromium

Technological properties

Property
Application areas

Electronic components (Opto discs). Transmitter and x-ray tubes, Photomultipliers, UV flame detectors/deuterium lamp, Lighting (Laser flash lamps, Purification/Germicidal UVC/UVB/UV-CCL lamps), Disinfection, Substrate Glass for wafer production.

Corrosion properties

Hydrolytic resistance Class HGB3 (ISO 719) - Acid resistance Class S4 (DIN 12116) - Alkali resistance Class A3 (ISO695)