Soda Lime Silicate Glass SCHOTT 8366

Alternative and trade names
SCHOTT 8366
Want to keep this datasheet? Save it now in your required format

Description

High electrical insulating general sealing glass

This material data has been provided by Schott Glass Tubing.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

2.61 g/cm³

Show Supplier Material materials with Density of 2.61 g/cm³

Thermal

PropertyValueTesting StandardComment

Annealing temperature

480.0 °C

Show Supplier Material materials with Annealing temperature of 480.0 °C

ISO 7884-4

Viscosity 10¹³ dPa·s

Coefficient of thermal expansion

9.2e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 9.2e-06 1/K

ISO 7991

mean value for 20-300 °C

Glass transition temperature

470 °C

Show Supplier Material materials with Glass transition temperature of 470 °C

ISO 7884-8

Softening temperature

675.0 °C

Show Supplier Material materials with Softening temperature of 675.0 °C

ISO 7884-3

Viscosity 10⁷·⁶ dPa·s

Specific electrical resistance temperature

280.0 °C

Show Supplier Material materials with Specific electrical resistance temperature of 280.0 °C

For ρ=10⁸ Ω·cm

Working temperature

1015.0 °C

Show Supplier Material materials with Working temperature of 1015.0 °C

ISO 7884-2

Viscosity 10⁴ dPa·s

Electrical

PropertyTemperatureValue

Electrical resistivity

250 °C

3.98e+06 Ω·m

Show Supplier Material materials with Electrical resistivity of 3.98e+06 Ω·m

350 °C

63096 Ω·m

Show Supplier Material materials with Electrical resistivity of 63096 Ω·m

Chemical properties

Property

Other

0.01 %

max., Lead, Cadmium, Mercury and Hexavalent Chromium

Technological properties

Property
Application areas

Glass suitable for bodies of glass electrodes (tubes for pH electrodes), Sealing glass for special lightning.

Corrosion properties

Hydrolytic resistance Class HGB3 (ISO 719) - Acid resistance Class S1 (DIN 12116) - Alkali resistance Class A2 (ISO695)