Description

Intermediate sealing glass to the glasses DURAN®, 8330, 8449, 8486, 8487 and tungsten.

This material data has been provided by Schott Glass Tubing.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

2.25 g/cm³

Show Supplier Material materials with Density of 2.25 g/cm³

Thermal

PropertyValueTesting StandardComment

Annealing temperature

560.0 °C

Show Supplier Material materials with Annealing temperature of 560.0 °C

ISO 7884-4

Viscosity 10¹³ dPa·s

Coefficient of thermal expansion

3.8e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 3.8e-06 1/K

ISO 7991

mean value for 20-300 °C

Glass transition temperature

510 °C

Show Supplier Material materials with Glass transition temperature of 510 °C

ISO 7884-8

Softening temperature

800.0 °C

Show Supplier Material materials with Softening temperature of 800.0 °C

ISO 7884-3

Viscosity 10⁷·⁶ dPa·s

Specific electrical resistance temperature

265.0 °C

Show Supplier Material materials with Specific electrical resistance temperature of 265.0 °C

For ρ=10⁸ Ω·cm

Working temperature

1210.0 °C

Show Supplier Material materials with Working temperature of 1210.0 °C

ISO 7884-2

Viscosity 10⁴ dPa·s

Optical

PropertyValueComment

Refractive index

1.5 [-]

Show Supplier Material materials with Refractive index of 1.5 [-]

at λ=587.6 nm

Technological properties

Property
Application areas

Transmitter and x-ray tubes, other Electrotechnology/Electronics

Corrosion properties

Hydrolytic resistance Class HGB1 (ISO 719)