Borosilicate Glass SCHOTT 8449

Alternative and trade names
SCHOTT 8449
Want to keep this datasheet? Save it now in your required format

Description

Intermediate sealing glass to the glasses FIOLAX® clear, 8412, 8447 and 8487.

This material data has been provided by Schott Glass Tubing.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

2.29 g/cm³

Show Supplier Material materials with Density of 2.29 g/cm³

Thermal

PropertyValueTesting StandardComment

Annealing temperature

550.0 °C

Show Supplier Material materials with Annealing temperature of 550.0 °C

ISO 7884-4

Viscosity 10¹³ dPa·s

Coefficient of thermal expansion

4.5e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 4.5e-06 1/K

ISO 7991

mean value for 20-300 °C

Glass transition temperature

535 °C

Show Supplier Material materials with Glass transition temperature of 535 °C

ISO 7884-8

Softening temperature

785.0 °C

Show Supplier Material materials with Softening temperature of 785.0 °C

ISO 7884-3

Viscosity 10⁷·⁶ dPa·s

Specific electrical resistance temperature

350.0 °C

Show Supplier Material materials with Specific electrical resistance temperature of 350.0 °C

For ρ=10⁸ Ω·cm

Working temperature

1150.0 °C

Show Supplier Material materials with Working temperature of 1150.0 °C

ISO 7884-2

Viscosity 10⁴ dPa·s

Optical

PropertyValueComment

Refractive index

1.5 [-]

Show Supplier Material materials with Refractive index of 1.5 [-]

at λ=587.6 nm

Technological properties

Property
Application areas

Transmitter and x-ray tubes, other Electrotechnology/Electronics