Borosilicate Glass SCHOTT 8487

Alternative and trade names
SCHOTT 8487
Want to keep this datasheet? Save it now in your required format

Description

Borosilicate glass for sealing to tungsten and high resistance to thermal shock.

This material data has been provided by Schott Glass Tubing.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

2.25 g/cm³

Show Supplier Material materials with Density of 2.25 g/cm³

Mechanical

PropertyValue

Elastic modulus

66 GPa

Show Supplier Material materials with Elastic modulus of 66 GPa

Poisson's ratio

0.2 [-]

Show Supplier Material materials with Poisson's ratio of 0.2 [-]

Thermal

PropertyTemperatureValueTesting StandardComment

Annealing temperature

560.0 °C

Show Supplier Material materials with Annealing temperature of 560.0 °C

ISO 7884-4

Viscosity 10¹³ dPa·s

Coefficient of thermal expansion

3.9e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 3.9e-06 1/K

ISO 7991

mean value for 20-300 °C

Glass transition temperature

525 °C

Show Supplier Material materials with Glass transition temperature of 525 °C

ISO 7884-8

Softening temperature

775.0 °C

Show Supplier Material materials with Softening temperature of 775.0 °C

ISO 7884-3

Viscosity 10⁷·⁶ dPa·s

Specific electrical resistance temperature

300.0 °C

Show Supplier Material materials with Specific electrical resistance temperature of 300.0 °C

For ρ=10⁸ Ω·cm

Thermal conductivity

90 °C

1.2 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 1.2 W/(m·K)

Working temperature

1135.0 °C

Show Supplier Material materials with Working temperature of 1135.0 °C

ISO 7884-2

Viscosity 10⁴ dPa·s

Electrical

PropertyTemperatureValueFrequency

Dielectric constant

4.9 [-]

Show Supplier Material materials with Dielectric constant of 4.9 [-]

1MHz

Electrical resistivity

250 °C

2e+06 Ω·m

Show Supplier Material materials with Electrical resistivity of 2e+06 Ω·m

350 °C

79433 Ω·m

Show Supplier Material materials with Electrical resistivity of 79433 Ω·m

Loss tangent

0.0036 [-]

Show Supplier Material materials with Loss tangent of 0.0036 [-]

1MHz

Optical

PropertyValueTesting StandardComment

Refractive index

1.5 [-]

Show Supplier Material materials with Refractive index of 1.5 [-]

at λ=587.6 nm

Stress optical coefficient

3.6e-06 mm²/N

Show Supplier Material materials with Stress optical coefficient of 3.6e-06 mm²/N

DIN 52314

Chemical properties

Property

Other

0.01 %

max., Lead, Cadmium, Mercury and Hexavalent Chromium

Technological properties

Property
Application areas

Engineering (Instruments / Barometers / Aerometers / Sightglasses), Electronic components, Lighting (Neon tubing, Flash lamps, Lamp bulbs, Exhust and Plate tubing, Laser flash lamps, other Lamps and Luminary). Camera- and Video components, Digital projection, Photodynamic therapy

Corrosion properties

Hydrolytic resistance Class HGB4 (ISO 719) - Acid resistance Class S3 (DIN 12116) - Alkali resistance Class A3 (ISO695)