Borosilicate Glass SCHOTT 8660

Alternative and trade names
SCHOTT 8660
Want to keep this datasheet? Save it now in your required format

Description

For sealing to tungsten, of high cesium content. High resistance to thermal shock and a longer life in comparison with glass 8487.

This material data has been provided by Schott Glass Tubing.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

2.44 g/cm³

Show Supplier Material materials with Density of 2.44 g/cm³

Thermal

PropertyValueTesting StandardComment

Coefficient of thermal expansion

4.1e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 4.1e-06 1/K

ISO 7991

mean value for 20-300 °C

Glass transition temperature

550 °C

Show Supplier Material materials with Glass transition temperature of 550 °C

ISO 7884-8

Softening temperature

830.0 °C

Show Supplier Material materials with Softening temperature of 830.0 °C

ISO 7884-3

Viscosity 10⁷·⁶ dPa·s

Specific electrical resistance temperature

550.0 °C

Show Supplier Material materials with Specific electrical resistance temperature of 550.0 °C

For ρ=10⁸ Ω·cm

Working temperature

1215.0 °C

Show Supplier Material materials with Working temperature of 1215.0 °C

ISO 7884-2

Viscosity 10⁴ dPa·s

Electrical

PropertyTemperatureValue

Electrical resistivity

250 °C

5.01e+10 Ω·m

Show Supplier Material materials with Electrical resistivity of 5.01e+10 Ω·m

350 °C

5.01e+08 Ω·m

Show Supplier Material materials with Electrical resistivity of 5.01e+08 Ω·m

Optical

PropertyValueComment

Refractive index

1.5 [-]

Show Supplier Material materials with Refractive index of 1.5 [-]

at λ=587.6 nm

Chemical properties

Property

Other

0.01 %

max., Lead, Cadmium, Mercury and Hexavalent Chromium

Technological properties

Property
Application areas

Red eye reduction flash for electronic flashbulbs and lighting, Camera- and Video components, Digital projection

Corrosion properties

Hydrolytic resistance Class HGB3 (ISO 719) - Acid resistance Class S3 (DIN 12116) - Alkali resistance Class A3 (ISO695)