General
Property | Value |
---|---|
Density | 2.34 g/cm³ Show Supplier Material materials with Density of 2.34 g/cm³ |
Mechanical
Property | Value |
---|---|
Elastic modulus | 73 GPa Show Supplier Material materials with Elastic modulus of 73 GPa |
Thermal
Property | Value | Testing Standard | Comment |
---|---|---|---|
Annealing temperature | 570.0 °C Show Supplier Material materials with Annealing temperature of 570.0 °C | ISO 7884-4 | Viscosity 10¹³ dPa·s |
Coefficient of thermal expansion | 5.5e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5.5e-06 1/K | ISO 7991 | mean value for 20-300 °C |
Glass transition temperature | 565 °C Show Supplier Material materials with Glass transition temperature of 565 °C | ISO 7884-8 | |
Softening temperature | 790.0 °C Show Supplier Material materials with Softening temperature of 790.0 °C | ISO 7884-3 | Viscosity 10⁷·⁶ dPa·s |
Specific electrical resistance temperature | 191.0 °C Show Supplier Material materials with Specific electrical resistance temperature of 191.0 °C | For ρ=10⁸ Ω·cm | |
Working temperature | 1175.0 °C Show Supplier Material materials with Working temperature of 1175.0 °C | ISO 7884-2 | Viscosity 10⁴ dPa·s |
Electrical
Property | Temperature | Value | Frequency |
---|---|---|---|
Dielectric constant | 5.9 [-] Show Supplier Material materials with Dielectric constant of 5.9 [-] | 1MHz | |
Electrical resistivity | 250 °C | 100000 Ω·m Show Supplier Material materials with Electrical resistivity of 100000 Ω·m | |
350 °C | 5012 Ω·m Show Supplier Material materials with Electrical resistivity of 5012 Ω·m | ||
Loss tangent | 0.0143 [-] Show Supplier Material materials with Loss tangent of 0.0143 [-] | 1MHz |
Optical
Property | Value | Testing Standard | Comment |
---|---|---|---|
Refractive index | 1.5 [-] Show Supplier Material materials with Refractive index of 1.5 [-] | at λ=587.6 nm | |
Stress optical coefficient | 3.3e-06 mm²/N Show Supplier Material materials with Stress optical coefficient of 3.3e-06 mm²/N | DIN 52314 |
Chemical properties
Property | ||
---|---|---|
Other | 0.01 % | max., Lead, Cadmium, Mercury and Hexavalent Chromium |
Technological properties
Property | ||
---|---|---|
Application areas | Renewable energies (Receiver), Fibre Optics | |
Corrosion properties | Hydrolytic resistance Class HGB1 (ISO 719) - Acid resistance Class S1 (DIN 12116) - Alkali resistance Class A2 (ISO695) |