SCHOTT GS10

Alternative and trade names
SCHOTT GS10
.XLSX
.PDF
Save

Description

Sealing glasses in general.

Properties

General

Density ρ

2.17 g/cm³ at 20 °C

Thermal

Annealing temperature Tanneal

725 °C

Viscosity 10¹³·² dPa.s (ISO 7884-4)

Coefficient of thermal expansion α

1.25E-6 1/K at 20 °C

mean value for 20-300 °C - ISO 7991

Softening temperature Tsoftening

1195 °C

Viscosity 10⁷·⁶ dPa.s (ISO 7884-3)

Specific electrical resistance temperature Tk

420 °C

For ρ = 10⁸ Ω·cm

Strain temperature Tstrain

635 °C

Viscosity 10¹⁴·⁷ dPa.s (ISO 7884-4)

Working temperature Tworking

1710 °C

Viscosity 10⁴ dPa.s (ISO 7884-3)

Electrical

Electrical resistivity ρel

3.16E+8 Ω·m at 250 °C

Show chart

Chemical properties

Element

Weight %

Comment

Si

85 %

SiO₂

B

10 %

B₂O₃

Al

4.5 %

Al₂O₃

Ba

0.5 %

BaO

Fe

0.1 %

max., Fe₂O₃

More

Technological properties

Application areas

Electronic Components, Signal intensifier, detector (other Electrotechnology/Electronics).

This material data has been provided by Schott Glass Tubing.