Borosilicate Glass SCHOTT GS30

Alternative and trade names
SCHOTT GS30
Want to keep this datasheet? Save it now in your required format

Description

Sealing glasses in general.

This material data has been provided by Schott Glass Tubing.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

2.24 g/cm³

Show Supplier Material materials with Density of 2.24 g/cm³

Thermal

PropertyValueTesting StandardComment

Annealing temperature

635.0 °C

Show Supplier Material materials with Annealing temperature of 635.0 °C

ISO 7884-4

Viscosity 10¹³·² dPa·s

Coefficient of thermal expansion

3.05e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 3.05e-06 1/K

ISO 7991

mean value for 20-300 °C

Softening temperature

1055.0 °C

Show Supplier Material materials with Softening temperature of 1055.0 °C

ISO 7884-3

Viscosity 10⁷·⁶ dPa·s

Specific electrical resistance temperature

440.0 °C

Show Supplier Material materials with Specific electrical resistance temperature of 440.0 °C

For ρ=10⁸ Ω·cm

Strain temperature

570 °C

Show Supplier Material materials with Strain temperature of 570 °C

ISO 7884-7

Viscosity 10¹⁴·⁵ dPa·s

Working temperature

1570.0 °C

Show Supplier Material materials with Working temperature of 1570.0 °C

ISO 7884-3

Viscosity 10⁴ dPa·s

Electrical

PropertyTemperatureValue

Electrical resistivity

250 °C

6.31e+08 Ω·m

Show Supplier Material materials with Electrical resistivity of 6.31e+08 Ω·m

350 °C

1.26e+07 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.26e+07 Ω·m

Technological properties

Property
Application areas

Electronic Components, Signal intensifier, detector and (fibre-) optics (other Electrotechnology/Electronics).